Uburyo bwo gusudira kumwanya wicyuma
gusudira :
Igikorwa cyo gusudira ninzira yingenzi mugukora ibyuma byumwanya wibyuma, kandi bigomba gukorwa muburyo bukurikije amabwiriza yo gusudira.Mugabanye impungenge zisigaye ziterwa no gusudira, kandi ukosore mugihe cyo guhindura uburyo bwo gushyushya umuriro.
A. Iyo umuyoboro wibyuma usudishijwe hamwe nicyapa gifunga hamwe nicyuma cyicyuma, igikoni kizakingurwa ukurikije ibisabwa, kandi impande ya groove igomba kuba yujuje ibisabwa byinguni ikozwe hagati ya electrode nubuso bwikariso kugirango birinde guhuzagurika kandi gushiramo.Mubyongeyeho, icyuho cya groove kigomba kuba kinini bihagije kugirango electrode arc igere munsi yigitereko kandi irinde ubujyakuzimu budahagije.
B. Irinde gushiraho icyuma cyo gusudira hagati yinkoni mugihe umuyoboro wibyuma usizwe.
C. Ibintu bikeneye kwitabwaho mugikorwa cyo gusudira:
a.Mugihe cyo gusudira intoki arc, intera yo kugemura ntigomba kuba nini cyane, kandi gusudira kwinshi-gutambuka.
Mugihe cyibikorwa, isaro yo gusudira cyangwa interlayer yo gusudira slag, gushyiramo slag, oxyde, nibindi bigomba kuvaho rwose.Gusya uruziga, ibyuma birashobora gukoreshwa.
Ibikoresho nka brush.
b.Ikidodo kimwe cyo gusudira kigomba gusudira ubudahwema kandi bikarangirira icyarimwe.
c.Kubice bitandukanye byo gusudira, nyuma yo gusudira birangiye, icyuma na spatter hejuru yicyuma bigomba gusukurwa.
Reba isura igaragara ya weld, kandi ntihakagombye kubaho kwiheba, isaro ryo gusudira, munsi, guhumeka, kubura fusion, gucamo
nizindi nenge zirahari.
d.Nyuma yo gusudira ikibuno, ultrasonic flaw detection igomba gukorwa nyuma yamasaha 24.